The March 2006 issue of PapierRestaurierung (vol. 7), the IADA
periodical on paper conservation, has now been published. The main
articles are:

    Jane L. Down, R. Scott Williams, Season Tse, Sherry Guild
    "The CCI Tapes and Heat-set Tissues Project-Description and
    Status Report" in English with German abstract: pp. 13-17

    Istvan Kecskemeti, Mika Seppala
    "False-colour Infrared (FCIR) Imaging-An Inexpensive Method for
    Identifying Iron-gall Ink by Standard Digital Camera" in English
    with German abstract: pp. 18-23

    Christina Meier
    "Schimmelpilze auf Papier-Fungizide Wirkung von Isopropanol und
    Ethanol" ("Moulds on Paper: Fungicidal Effect of Isopropanol and
    Ethanol") in German with English abstract: pp. 24-31

    Doreen Weiss
    "Ethanol und Chlormetakresol als Fungizide-Auswirkungen auf die
    Alterungsbestandigkeit von Papier"
    ("Ethanol and Chlormetakresol as Fungicides: Effects on the
    Durability of Paper") in German with English abstract: pp. 32-40

Further it contains shorter contributions (in german) under the
headings: Editorial, IADA inside, Materials and Equipment,
Literature, Further Education.

All titles, abstracts, links can be found at
    <URL:http://palimpsest.stanford.edu/iada/pr0106_t.html>

Information and orders:

    Fototext Publishing House
    Wolfgang Jaworek
    Liststr. 7 /B
    70180 Stuttgart
    Germany
    Fax: +49 711 609024
    ISSN: 1563 2628

FotoText Verlag Wolfgang Jaworek
Liststrasse 7/B
70180 Stuttgart
Germany
+49 711 609021
Fax: +49 711 609024


                                  ***
                  Conservation DistList Instance 19:44
                 Distributed: Thursday, March 16, 2006
                       Message Id: cdl-19-44-008
                                  ***
Received on Tuesday, 7 March, 2006

[Search all CoOL documents]


URL: http://
Timestamp:
Retrieved: