Subject: Microballoon mixture for wood

Microballoon mixture for wood

From: Denise Troughton <denise.troughton>
Date: Tuesday, March 14, 2006
Eugenia Stamatopoulou <stamatopoulou [at] deste__gr> writes

>This query is posted on behalf of Maria Filipoussi
>
>    Does anybody have information about epoxy resin/phenolic
>    microballoons mixture as a filler for wood objects? I am looking
>    for a commercial brand name and suppliers in Europe.

West Systems is the trade name of a marine epoxy resin with option
of microballoons - check with your local chandlery or marina (used
on repair and restoration of wooden boats)

Denise Troughton