Eugenia Stamatopoulou <stamatopoulou [at] deste__gr> writes

>This query is posted on behalf of Maria Filipoussi
>
>    Does anybody have information about epoxy resin/phenolic
>    microballoons mixture as a filler for wood objects? I am looking
>    for a commercial brand name and suppliers in Europe.

You can find the microballoons at:

    SP System Ltd
    St Cross Business Park
    Newport IOW PO30 5WU.

There's an excellent article written on 'The mechanical behaviour of
adhesives and gap fillers for re-joining panel paintings in the
National Gallery Technical Bulletin, vol.23, by Christina Young,
Paul Ackroyd, Roger Hibberd and Stephen Gritt.

Vera Blok
Intern paintings conservator Mauritshuis, The Hague


                                  ***
                  Conservation DistList Instance 19:44
                 Distributed: Thursday, March 16, 2006
                       Message Id: cdl-19-44-003
                                  ***
Received on Tuesday, 14 March, 2006

[Search all CoOL documents]


URL: http://
Timestamp:
Retrieved: