Victoria Montana Ryan <eltacorey [at] worldnet__att__net> writes

>I have a query from an allied professional.  They are considering
>using the UV filtering film V-Cool on the windows of a historic
>structure, where they have previously used plexiglas.  Understanding
>that the "lifetime" of either material is, on average about 12
>years, they are concerned that after application of the film to the
>original glazing, removal might cause damage. ....

If you replace the plexi with 1/4 inch laminated glass, you will get
added strength, clarity, protection and UV protection all at the
same time.

Victor Rothman
1468 Midland Ave #5
Bronxville, N.Y. 10708


                                  ***
                  Conservation DistList Instance 19:14
               Distributed: Saturday, September 10, 2005
                       Message Id: cdl-19-14-005
                                  ***
Received on Saturday, 3 September, 2005

[Search all CoOL documents]


Feedback for CoOL webmaster