Tiziana Lanave <athosnave [at] yahoo__it> writes

>I am working on the design of a conservation lab for treatment of
>waterlogged wood and am looking for all information about
>establishing a lab ...

I published a short paper titled "Archaeological Conservation
Laboratory Design--A Parks Canada Solution" in the Proceedings of
the 8th ICOM Group on Wet Organic Archaeological Materials
Conference which took place in Stockholm in 2001.  The book was
published by the International Council of Museums (ICOM), Committee
for Conservation Working Group on Wet Organic Materials in
Bremerhaven in 2002.  The editors were Per Hoffmann, James A.
Spriggs, Tara Grant, Clifford Cook and Andrea Recht.  ISBN
3-933885-11-6.

Clifford Cook
Project Development Advisor
Canadian Conservation Institute
1030 Innes Road
Ottawa, Ontario
K1A 0M5 Canada
613-998-3721 #152
Fax: 613-998-4721


                                  ***
                  Conservation DistList Instance 19:10
                Distributed: Wednesday, August 17, 2005
                       Message Id: cdl-19-10-016
                                  ***
Received on Monday, 15 August, 2005

[Search all CoOL documents]


Feedback for CoOL webmaster