Hartmut Kutzke <h.kutzke [at] uni-bonn__de> writes

>We are working on the conservation of a Tapa from Hawaii. Do anyone
>have information about the impregnation (oils, waxes, resins etc.)
>of such tapas? And on the binding media for pigments used in
>traditional Hawaiian artcraft? Furthermore, we are looking for a IR
>spectrum of candlenut.

A belated note on tapa: you might contact Val Free, at the Bishop
Museum vfree<-a t->bishopmuseum< . >org

Kent Severson
Conservator in Private Practice
74 The Fenway, #43
Boston, Massachusetts  02115
617-267-9093


                                  ***