Mark Vine <vpackthread [at] aol__com> writes

>A conservator without access to the Internet has asked for advice on
>what might be suitable for filling a gaping hole in an antler.

You could just cut and turn a simple honest elegant plug made from
another antler, set in glue made from the same or the hide, if
necessary. If a filler is needed you could use the chips and sawdust
from modelling the plug? Why introduce alien material?