Adam Barr <abarr [at] jcu__edu> writes

>I am looking for a source in the US for humidity controlled display
>cases for home use. ....

Glasbau Hahn produces humidity controlled display cases in an active
and passive way. Passive is the humidity control with silica gel. The
active control can be achieved with a small humidifier, which
constantly injects purified and conditioned air into the display
case. Glasbau Hahn is based in Germany, but there are two offices in
the US which distribute the display cases there: One in the west,
near Los Angeles, called

    Glasbau Hahn America
    984 Monument Street, Suite 201
    Pacific Palisades CA 90272
    310-317-0334

and one office in New York city

    25 West 64th Street
    New York NY 10023
    212-721-6183

You can view some humidified cases at
    <URL:http://www.glasbau-hahn.de/
        english/vitrinen/reinluft/reinluft_en.php>

    **** Moderator's comments: The above URL has been wrapped for
    email. There should be no newline

Isabel Hahn
Glasbau Hahn
Display case manufacturer
Hanauer Landstrasse 211
D - 60314 Frankfurt am Main



                                  ***
                  Conservation DistList Instance 16:30
                Distributed: Wednesday, October 30, 2002
                       Message Id: cdl-16-30-012
                                  ***
Received on Monday, 28 October, 2002

[Search all CoOL documents]


Feedback for CoOL webmaster