Subject: Adhesives for Ethafoam

Adhesives for Ethafoam

From: Mark Vine <100436.3447>
Date: Friday, September 13, 2002
Jerry Fahey <jfahey [at] siue__edu> writes

>Over the years I've used hot glue or water based contact cement to
>adhere Ethafoam for shipping crate packing and collection padding.
>Well, being the 21st century, I'm trying to find something a little
>easier to use. I got in touch with the adhesive folks at 3M and they
>suggested one of their Adhesive Transfer Tapes, #950. It's made
>specifically for adhering foam products.

Another 3M product which Jerry Fahey might wish to look at is
"465",a medium-firm completely clear acrylic adhesive transfer tape
product. We offer this item in a 25 mm (1") by 55 metre roll length.

"465" was designed as an alternative to the many harmful off-gassing
hot melt adhesive systems in use,as a more conservation friendly
system for adhering polyethylene foam products such as plastazote
and ethafoam to other substrates.

"465" has excellent UV light resistance and a high solvent
resistance, it can be used to bond similar and dissimilar materials
such as metals, glass and plastics together.

It does have to be remembered that unlike other adhesive systems
"465" is not easily reversible in the normal manner.

For a sample and further size details contact either our location
here in the UK or Conservation Resources International, Springfield,
Virginia.

Mark G. Vine
Conservation Resources (UK) Ltd
England
Fax: +44 1865 747035


                                  ***
                  Conservation DistList Instance 16:20
                Distributed: Monday, September 16, 2002
                       Message Id: cdl-16-20-007
                                  ***
Received on Friday, 13 September, 2002

[Search all CoOL documents]


Feedback for CoOL webmaster