Just experimenting with a  product I just found, Mrs. Cooper's
Silver Wipes. Dampened with water, it gave a very nice gentle clean.
Easy to control and remove.  The press releases say that it is
silicone-based.  The company will not divulge the ingredients.
Anyone out there know anything about this product?  It was actually
fun to use (if cleaning silver can ever be fun).