Conservation DistList Archives [Date] [Subject] [Author] [SEARCH]

Subject: Solarization of glass

Solarization of glass

From: Mary Fahey <maryf>
Date: Thursday, August 1, 2002
I am interested in obtaining information regarding the solarization
of glass. Specifically I would like to know if it should be a
consideration in terms of limiting light levels in glass displays.
I'd appreciate any information regarding this subject.

    **** Moderator's comments: For those who, like me, were
    unfamiliar with the term "solarization" as it pertains to glass,
    see <URL:http://www.uvp.com/pdf/a112.pdf> for an explanation.

Mary Fahey
Chief Conservator/ Head of Preservation
Henry Ford Museum and Greenfield Village
20900 Oakwood Blvd
Dearborn, Michigan 48121
313-982-6072


                                  ***
                  Conservation DistList Instance 16:11
                  Distributed: Friday, August 2, 2002
                       Message Id: cdl-16-11-013
                                  ***
Received on Thursday, 1 August, 2002

[Search all CoOL documents]