Subject: Marvel Century anti-tarnish paper

Marvel Century anti-tarnish paper

From: Colin L. Leci <iceldevp>
Date: Tuesday, January 8, 2002
Martha Singer <martha_singer [at] hotmail__com> writes

>Does anyone know if Marvel Century anti-tarnish paper is still made,
>who fabricates it and where it can be purchased? I have a telephone
>number (201-485-4400) which is no longer in service.

If this is to prevent attack from sulphur species you could use
Miracle Sac supplied by ICEL Developments Ltd UK


                                  ***