Georgianne Bowman <ggbowman [at] email__msn__com> writes

>We are a small historical society which has recently acquired a
>small museum space.  The building is in need of renovation.  We are
>aware that we need temperature and humidity control and this will be
>dealt with in the remodeling.

You may wish to consider using a Micro Climate Generator to feed a
constant flow of tempered air to your exhibit cases. The Constant
Volume Generator supplies tempered air through a small hose to up to
6000 cubic feet of display or storage cabinets. As there is constant
positive pressure, the cases can be "leaky" and still maintain the
correct humidity. The MCT system will ensure constant humidity
levels in the cases regardless of temperature and moisture
variations in the museum space, and will also "flush" off-gassing
from the case and enclosed objects. More information and links may
be found at <URL:http://www.gowncare.com/keepsafe>

Jerry Shiner
Keepsafe Systems
Micro-climate and Oxygen-free storage for Professional Conservators
800-683-4696
Fax: 416-703-5991


                                  ***
                  Conservation DistList Instance 14:50
                 Distributed: Wednesday, March 28, 2001
                       Message Id: cdl-14-50-005
                                  ***
Received on Saturday, 24 March, 2001

[Search all CoOL documents]


URL: http://
Timestamp:
Retrieved: