For those interested in removing surface marks and blemishes from
acrylic sheeting we have just added a lightweight mini electronic
polisher. The LH16E runs at 700 to 1700 revolutions and weighs a
mere 1.9 kilos making it one of the lightest electrically powered
polishers around. The unit has been introduced to complement our
range of perspex cleaning solutions.