J. Claire Dean <clairedean [at] aol__com> writes

>Does anyone have a source for papyrus?

I have bought it at regular art supply stores, and also, I think,
from the Flax Art catalog. Calligraphers still use it, so it's
fairly available. I haven't seen the loose materials though.