In response to Brad Cole's question about the clogging of Wei T'o
equipment:

First of all, clean the gun, and perhaps the hoses, with vinegar to
remove all deposits.

When you are finished spraying the Soft Spray, run cleaning solution
through the system in the normal way.  Make sure all of the Soft
Spray is expelled.  Instead of emptying the line of all cleaning
solution, leave the lines full of cleaning solution, and also
back-flush cleaning solution up into the Soft Spray line (the short
hose between the "T" valve and the Soft Spray tank).  Before your
next use, spray out the cleaning solution in the hoses and then open
the Soft Spray valve.

This procedure was suggested by the manufacturer some time last
year, and has proved successful for us since that time.  Also, at
that time we replaced our hoses (and all fittings and valves) with
the new clear hoses which seem to work well, and allow you to see
the solution in the lines.

Harry Campbell
Conservation Division
Information Conservation, Inc.

                                  ***
                  Conservation DistList Instance 9:62
                 Distributed: Thursday, March 14, 1996
                        Message Id: cdl-9-62-011
                                  ***
Received on Monday, 11 March, 1996

[Search all CoOL documents]


URL: http://
Timestamp:
Retrieved: