Just to add more information to the removable tape/sticky tab arena,
Robin Siegel presented a paper, "The Conservation Implications of Yellow
Sticky Tabs" at the 1989 Winter meeting of the Photo Materials Group of
AIC which addressed some of the concerns in using these materials.
Essentially she researched the warning that is printed on post-it note
packaging which states "May leave a mark on some surfaces and lift ink.
Test before using on questionable paper." For anyone interested in
reading up on this, Robin's paper can be found in:  "Topics in
Photographic Preservation" volume 3. American Institute for
Conservation, Photographic Materials Group, 1989. pp. 66-8.

Deborah Derby

                                  ***
                  Conservation DistList Instance 8:45
                 Distributed: Sunday, December 11, 1994
                        Message Id: cdl-8-45-003
                                  ***
Received on Thursday, 8 December, 1994

[Search all CoOL documents]


Feedback for CoOL webmaster