Scott Petersen <scpeters [at] alexandria__lib__utah__edu> writes

>Does anyone know of a
>different, less damaging, way to remove spine labels stamped in gold,
>silver and black?

At the University of Michigan bindery we used blue household ammonia
with a toothbrush to remove gold stamping from pyroxylin-coated book
covers.  It worked fine.