Sue, if you use B72, be sure to use it from toluene to get maximum
adhesion (see Eric Hanson's article on alteration of physical properties
of pva films cast from various solvents in JAIC; he followed this year
with B72 at the AIC conference. Good work, and nicely confirms
experiential knowledge).

is emu as thick as ostrich? I would be tempted to use Epotek myself if
not, and if handling is foreseen....