Ozone generators do indeed remove odors including mold and mildew. Most
"disaster response" firms use the ozone generators after the cleaning
process is complete, not to control mold.  Dehumidification and
temperature are the current stabilizing treatment for mold, after it has
been removed. The drawback with using ozone is that it makes the paper
brittle with prolonged exposure.  3-4 hour exposure is recommended.

                                  ***