Conservation DistList Archives [Date] [Subject] [Author] [SEARCH]

Subject: Standard for permanent paper

Standard for permanent paper

From: Hilary A. Kaplan <bm.gsk>
Date: Friday, March 12, 1993
The new ANSI Standard for permanent paper, Z39.48-1992 has, in fact,
been approved and may be referred to as such.

                                  ***