To Paper Technologies, Inc. Customers:
 
It has been brought to our attention that, due to a mix-up at the mill,
some of the papers which were received of P.T.I.-Wove Endleaf contained
batches of papers which are not acid-free and, therefore, do not meet
with our requirements.
 
The following colors are questionable:
 
   1)  Creme      2) Ivory     3)  Misty Grey
 
If any of the above colors were received by you, we ask you not to use
this paper.  Please discard it.
 
We will reimburse you for any  shipments which were made or, if you
prefer, we will make arrangement for replacement with any of the
following colors:
 
#4 Lavender Blush,  #5 Vanilla,  #6 Cafe au Lait, # 7 Soft Grey
 
We sincerely regret any inconvenience which may have been caused to you
by this.  We will be arranging for new productions of the 3 colors
listed above and will let you know as soon as they are available.
 
All customers that purchased these colors will be contacted by
phone/mail.
 
Paper Technologies, Inc.
 

                                  ***
                  Conservation DistList Instance 6:43
                Distributed: Thursday, February 4, 1993
                        Message Id: cdl-6-43-001
                                  ***
Received on Thursday, 4 February, 1993

[Search all CoOL documents]


Feedback for CoOL webmaster