>Does anyone have any experience with the use of Fuji film for
>preservation microfilming?
>Sara Williams

We have been shooting Fuji for some years, based upon the cost
advantage. We have no reason to be dissatisfied.  However, do order the
HRII PET125, which is the polyester base.  The 1987 announcement on
triacetate dimensional shrinkage caused us to change in a hurry.

Michael McCormick
Western Reserve Historical Society

                                  ***