3M made paper-based tapes in 1947 and 1948.  I'm sure other companies used
paper.  I don't like it because it tears so easily.

Jim Wheeler

Jim Wheeler wrote:

>3M made paper-based tapes in 1947 and 1948.  I'm sure other companies used
>paper.  I don't like it because it tears so easily.

Didn't Brush make paper tape?