What are the recommended temperatures and "baking time" for
tapes? I have heard that a longer baking time (100 - 120 hours)
at lower temperatures of 50=B0C is preferable to a shorter baking
time of 9 hours at the higher temperature of 70=B0C. Within what
time span do the tapes start disintergrating again after baking?
Does a longer baking time help prolong this interval?