Polyline has sent us a sample of their polypropylene CD storage sleeve. It
has a compartment for the CD and another compartment for documentation. We
like it. But is it "archival?"
It has a "patented, white non-woven" divider between the two compartments.
Polyline can't tell us what this material is made of. It could be a piece of
paper? Is it acidic? Has anyone else looked at this product?