Yes, running the tape from end to end at high speed will reduce
print-thru somewhat, according to 3M.  Not exactly a cure, but
every little bit helps.

Doug

This is called "print through" where the signal on one layer of a=20
tape impresses itself onto adjacent layers of the tape. In rare=20
instances, you can hear things repeat more than once.

The time difference between the original and the image is once around
the reel.

Sometimes this can be cured by winding the tape through and letting=20
it sit for a few days.