Re: [ARSCLIST] SSS Agfa [WAS: Ampex 456 and Shamrock 041 Manufacturing Specs?]



I used 469 for all of my mixing during the mid '80s. Thankfully we had run
Sony PCM-F1 backups of everything we kept.


Bob Olhsson Audio Mastery, Nashville TN
Mastering, Audio for Picture, Mix Evaluation and Quality Control
Over 40 years making people sound better than they ever imagined!
615.385.8051 http://www.hyperback.com    http://www.thewombforums.com



> -----Original Message-----
> From: Association for Recorded Sound Discussion List
> [mailto:ARSCLIST@xxxxxxx] On Behalf Of Marie O'Connell
> Sent: Friday, February 27, 2009 3:59 AM
> To: ARSCLIST@xxxxxxxxxxxxxxxx
> Subject: Re: [ARSCLIST] SSS Agfa [WAS: Ampex 456 and Shamrock 041
> Manufacturing Specs?]
> 
> To give Agfa some credit, I was always told that in the late 1980's,
> early
> 1990's, there was a worldwide recall of this tape and our archive did
> take
> advantage of this and sent some 300 10.5 reels, all paid for by them.
> We
> were sent back re-mastered 'copies on new stock.  When I am back at
> work I
> can check the 'new' brand of stock.  Needless to say, accessions we get
> in
> to this day still have this PEM 469, broadcasters etc who never knew
> about
> this recall.
> 
> 
> 
> On Fri, Feb 27, 2009 at 10:06 PM, Tommy Sjöberg <
> tommy.sjoberg@xxxxxxxxxxxxxxxxxx> wrote:
> 
> > Hi all,
> >
> > I worked on a digitizing project for Universal music some years ago,
> doing
> > several thousand tapes. I totally agree about Ampex 456 - the few we
> didn't
> > bake sure smelled like they would need baking, but weren't shedding,
> just
> > yet.
> >
> > We never encountered a Basf tape that needed baking, and the same for
> Agfa
> > with one, big exception and that is PEM 469, until they changed the
> > formulation sometime around 1990. All earlier 469's were baked. A few
> 468's
> > were also a bit sticky and were baked and then played fine, but if
> that was
> > SSS I don't know.
> >
> > Regards,
> >
> > Tommy Sjöberg
> > Folkmusikens hus
> > Rättvik, Sweden
> >
> >
> >
> >
> >> Date:    Thu, 26 Feb 2009 12:06:06 -0000
> >> From:    "Prentice, Will" <Will.Prentice@xxxxx>
> >> Subject: SSS Agfa [WAS: Ampex 456 and Shamrock 041 Manufacturing
> Specs?]
> >>
> >> Hi Goran
> >>
> >> Thanks for the info. Re. Agfa, we've had several examples of PE 49
> >> (double play, 7") which have proven sticky. According to the numbers
> in
> >> the green leader tape there were two manufactured bad batches at
> least,
> >> both seemingly bought by us at the same time, circa mid-1988. The
> >> numbers to beware of are 01041 and 15383. All other PE 49 batches
> thus
> >> far have been fine.
> >>
> >> Regards
> >>
> >> Will
> >> -----Original Message-----
> >> From: Association for Recorded Sound Discussion List
> >> [mailto:ARSCLIST@xxxxxxx] On Behalf Of Goran Finnberg
> >> Sent: 25 February 2009 12:38
> >> To: ARSCLIST@xxxxxxxxxxxxxxxx
> >> Subject: Re: [ARSCLIST] Ampex 456 and Shamrock 041 Manufacturing
> Specs?
> >>
> >> Will Prentice:
> >>
> >>  > Responding to Richard's comment that "all tape
> >>  > manufacturers seemed to have created batches of
> >>  > tape which suffered from this [i.e., SSS]"
> >>
> >> I have never ever seen any BASF tape ever go sticky shed.
> >>
> >> BASF is one of the worlds biggest chemical companies.
> >>
> >> They have always claimed that they had all the knowldedge in house
> >> together with making all the ingredients in house.
> >>
> >> So their position is that due to the above none of their tapes will
> >> exhibit sticky shed as they knew how to avoid it.
> >>
> >> AGFA, it is the same except for some batches of Agfa 468 during half
> a
> >> year or so.
> >>
> >> I have only seen one real of 468 go sticky despite having
> transferred
> >> several hundred such reals over the years.
> >>
> >> In contrast it is almost a given that any reel of Ampex 456 will go
> >> sticky for sure.
> >>
> >> And that is true over here since so far they all need baking.
> >>
> >>
> >> --
> >> Best,
> >>
> >> Goran Finnberg
> >> The Mastering Room AB
> >> Goteborg
> >> Sweden
> >>
> >> E-mail: mastering@xxxxxxxxx
> >>
> >> Learn from the mistakes of others, you can never live long enough to
> >> make them all yourself.    -   John Luther
> >>
> >