[Table of Contents]


[Date Prev][Date Next][Thread Prev][Thread Next][Date Index][Thread Index]

[ARSCLIST] Moldy Tapes



Hi All,

Got two boxes of moldy (purty deep forest green) 1/4 inch reels (some backcoated) that need to be cleaned up, transferred and reboxed.  Is there a good method for physically getting the mold off the oxide layer that doesn't involve foot by foot wiping?  Passing through a dry cloth gets the surface stuff off but even two passes of wet/dry doesn't get the adhered layer off the magnetic surface.  

Martin


[Subject index] [Index for current month] [Table of Contents]