> In the current high-end catalog, Musicdirect, a record flattening machine is
offered. It's at the bottom of p. 30 and called "Air Tight DT-01." Anyone have
experience with it?
>
> I can't find a manufacter on the net so can't ask him questions. How does it
work on 78s is the big one.
>
Assuming it "flattens" warped records...shellac 78's are actually
quite easy to unwarp...they become flexible at a fairly low
temperature.
However, flattening warped vinyl records would be much more of a
challenge, since the warping seems to be caused by the plastic
actually growing when subjected to heat...?!