[Date Prev][Date Next][Thread Prev][Thread Next][Date Index][Thread Index]
Re: [ARSCLIST] scotch 227
Try holding a cotton swab soaked in Isopropyl alcohol on the recorded side
of the tape before it passes through the tape guides and heads. The cotton
swab should be just damp and has to be applied continually while the tape is
running. This usually eliminates the screech.
Gary Higgins
The Living Word
-----Original Message-----
From: Association for Recorded Sound Discussion List
[mailto:ARSCLIST@xxxxxxx] On Behalf Of Bridavsky, Michael G
Sent: Thursday, March 30, 2006 8:27 AM
To: ARSCLIST@xxxxxxxxxxxxxxxx
Subject: [ARSCLIST] scotch 227
Hello,
I've been reading the list for while and appreciate the information and
knowledge that is shared here, and I have a question about a particular
brand/stock of tape.
Most of our recordings made in the mid-late 80's and easrly 90's was
recorded to Scotch 226. It's all pretty sticky, but bakes well. I have
just encountered a single reel of Scotch 227. It seems to be a thinner
tape than the 226, ad Im assuming it was an economy version of 226. It
is also sticky, however it does not respond to baking. While the amount
of deposit left on the heads and guides is minimal, and the tape passes
through the transport without slowing, the squeal and distortion is
audible in the transfer.
Does anyone have any experience with this tape? Any suggestions or other
treatments that might get it to run smoothly?
Thanks
mike
----------------------------------
Michael Bridavsky
Audio Engineer
Digital Audio Archiving Project
Indiana University School of Music
Office: 812-855-6061
Cell: 812-327-7939