Hello Martin,
I have received a number of CDs in sleeves made of vinyl similar to the
one you are investigating. Any flexible plastic sleeves are kept pliant
by volatile plasticizers which will migrate over time. Remember the
double pocket carriers that Brodart used to sell to libraries-album in
one side, disc in heavy sleeve in the other? They stick together very
affectionately and cause hazing of the LPs if left undisturbed for
several years (as will be the case with the material you have.)
 

David J. Diehl
Library Director
Texas State Technical College