on 8/10/05 1:36 AM, Lou Judson at inaudio@xxxxxxxxxxx wrote:

> I always burn a "CD24" aiff CDROM as well for archiving my projects. I
> believe there will be a better chance of readibility down the road...

For us it's really a matter of practicality. On some days we might have 4
recitals back to back. As much as we'd like to, there simply is not enough
time to burn CD 24s as well.

--
Konrad Strauss
Director of Recording Arts
Associate Professor of Music
Indiana University School of Music