CD discs are not laminated as DVD discs are. CD discs do not use any
adhesive. After the CD disc is molded and metallized, a very thin protective
layer is spin-coated over the metallization.

Jerry
Media Sciences, Inc.

> -----Original Message-----
> From: Association for Recorded Sound Discussion List
> [mailto:ARSCLIST@xxxxxxx] On Behalf Of Bev Lambert
> Sent: Wednesday, July 06, 2005 10:26 AM
> To: ARSCLIST@xxxxxxxxxxxx
> Subject: [ARSCLIST] delamination of CDs
>
> I am not a preservation scientist or even an knowledgeable audiophile, but
> an archives conservator charged with the task of researching best
> practises for digitization of magnetic media.  So, my question may seem
> naive: is it known whether CDs are laminated with an adhesive?  and if so,
> is it known which adhesive this is?  It seems to me that a different
> process. such as heat or pressure lamination would be more appropriate?
> Bev Lambert, Archives Conservator
> Provincial Archives at The Rooms
> St. John's, Newfoundland, Canada


[Subject index] [Index for current month] [Table of Contents]