And, by all means, keep them in a dark place.

Steve Smolian

----- Original Message -----
From: <Joe_Iraci@xxxxxxxxx>
To: <ARSCLIST@xxxxxxxxxxxx>
Sent: Thursday, March 10, 2005 11:45 AM
Subject: Re: [ARSCLIST] Temperature Requirements for CDs and digital media


There is an ISO standard (ISO18925 2002) that does provide some general
recommendations. The following are taken directly from the standard:

Relative Humidity (RH) should be between 20 and 50%.

Cycling of RH should not be greater than plus/minus 10%

Maximum temperature for extended periods should not exceed 25 degrees C.

Temperatures below 23 degrees C are preferable.

Peak temperature should not exceed 32 degrees C.

Useful life will be increased by storing discs at low temperature and low
relative humidity, since chemical degradation is reduced at these
conditions. Storage of discs below   -10 degrees C and below 10% RH is not
recommended.
---------------

Note if storing discs at cool or cold temperatures, ensure they are
packaged correctly in order to avoid moisture condensation on the discs as
they warm up to use conditions.


Joe Iraci Senior Conservation Scientist Canadian Conservation Institute



            Christina
            Hostetter
            <chostetter@PRESS                                          To
            .ORG>                     ARSCLIST@xxxxxxxxxxxx
            Sent by:                                                   cc
            Association for
            Recorded Sound                                        Subject
            Discussion List           [ARSCLIST] Temperature Requirements
            <ARSCLIST@xxxxxxx         for CDs and digital media
            >


10/03/2005 11:04 AM


Please respond to Association for Recorded Sound Discussion List <ARSCLIST@xxxxxxx >






Can anyone tell me what, if any optimal conditions are required for CDs and digital media? I know there are specific temperature requirements for magnetic media and film but I don't know if there are any conclusive recommendations for digital formats. Is there an answer to this question?

~~~~~~~~~~~~~~~~~~~~~~~~~
Christina J. Hostetter
Archivist/Research Librarian
Eric Friedheim Library at the
National Press Club
529 14th Street, NW
Washington, DC  20045
Tel: (202) 662-7523
Fax: (202) 879-6725
www.press.org/library/archives
~~~~~~~~~~~~~~~~~~~~~~~~~


-- No virus found in this incoming message. Checked by AVG Anti-Virus. Version: 7.0.308 / Virus Database: 266.6.4 - Release Date: 3/7/2005





-- No virus found in this outgoing message. Checked by AVG Anti-Virus. Version: 7.0.308 / Virus Database: 266.6.4 - Release Date: 3/7/2005


[Subject index] [Index for current month] [Table of Contents]