In a message dated 3/3/2005 8:34:40 AM Eastern Standard Time,
arclists@xxxxxxxxxxxxxxx writes:
Since SSS has happened, we've been told that it was just coincidental
that back
coating and the "bad" binder formulation happened at the same time.
************

I was told by one tape manufacturer back in the 70s that their back coating
was essentially the same as the active coating, just less controlled and with a
different finishing operation. Therefore it would contribute to the SSS
problem.

Mike Csontos