Don Cox wrote:

> Paraffin wax comes in a range of different melting points.
> Which do you recommend?

The kind of wax sold in grocery stores for home canning sealing works well.



... Graham Newton

--
Audio Restoration by Graham Newton, http://www.audio-restoration.com