FINDING SUBSTITUTE SURFACTANTS FOR SYNPERONIC N
JOHN A. FIELDS, ANDREW WINGHAM, FRANCES HARTOG, & VINCENT DANIELS
12 CONCLUSIONS
Evaluation of the results of the washing studies shows that five surfactants are suitable as substitutes for Synperonic N. These are the anionic surfactants Hostapon T and Orvus WA paste and the nonionic surfactants Dehypon LS45, Imbentin C135/070, and
Table .
Product Data of Five Surfactants Selected as Substitutes for Synperonic N (n/a = not applicable)
![](../img/jaic43-01-005-ch5tb7.gif) |
Synperonic 91/6. As the cloud point of Dehypon LS45 is 20–22�C, it should not be used at more than about 2�C above that temperature.
|