WATER-STAINED CELLULOSICS: A LITERATURE REVIEW
J.K Hutchins
ABSTRACT—This report describes published research that analyzes and explains phenomena familiar to those who work with water-stained cellulosic fabrics and paper, and that suggests a new line of inquiry in the study of foxing.