RESTORATION OF A LARGE CHINESE BRONZE URN
Aron A. Apisdorf
7 NEARLY THREE YEARS LATER
At this time, the urn was inspected. Under very close observation, no deterioration is in evidence and the urn's condition has not altered in any way (Fig. 6).