ERADICATION OF INSECTS FROM WOOL TEXTILES
Barbara M. Reagan
ABSTRACT—A variety of chemical and nonchemical methods is available for controlling fabric pests. Part I in this series presents an overview of the various methods available for insect control on wool textiles. Part II presents the results of a study on the feasibility of using microwaves as a nonchemical means of insect control.