Bookbinding and the Conservation of Books
A Dictionary of Descriptive Terminology

 Previous item  Up One Level Next item

split hide

The outer or grain layer of a hide from which the under or flesh side has been removed to produce a reasonably uniform thickness of less substance than the entire hide. The resultant leather is generally slightly thicker than 1.5 mm. (351 )