raspail test

A method of determining the presence of rosin size in paper. One drop of a strong solution of ordinary sugar is applied to the sheet, the excess being blotted after one minute. A drop of concentrated sulfuric acid is then applied, which turns the area treated a bright red color if rosin is present in the paper. (143 )