cornerpiece ( cornerstamp )

1. A bookbinding finishing tool, usually ARABESQUE , designed to be used at the corners of a leather binding, usually for the purpose of matching a centerpiece or other form of decoration. 2. Metal corners attached to a binding to protect the corners of the covers from damage. Removable pasteboard cornerpieces are sometimes used to protect the corners of books during shipment. (156 , 310 )