copolymer

A complex polymer, resulting from the polymerizing together of two or more different monomers or monomer combinations. A copolymer is a true compound and often has properties distinct from those expected of a physical mixture of the separately polymerized component monomers. An example of an important copolymer used in archival work is the vinyl chloride-vinyl acetate copolymer.