chevrotain

A leather produced from the skin of any of several very small deer-like mammals of Asia and West Africa, and used in England, principally in the Middle Ages, for chemises. Like the skins of does, lambs and other very young animals, it is soft and supple. It is sometimes inaccurately referred to as CHEVRETTE . (115 )