catalog paper

A lightweight paper, either coated or with an English finish, usually made with a considerable proportion of mechanical pulp, and used for mail-order catalogs, telephone directories, and the like. Uniformity of weight, opacity. finish, formation, and sufficient strength to get through high-speed printing presses are desired characteristics. Basis weights usually range from 19 to 28 pounds (24 X 36�). (17 , 324 )