armorial bearings

Solid plates of brass, engraved in relief with family heraldic insignia, and used to block insignia on the covers of books belonging to prominent and/ or royal families. Armorial bearings have been seldom used in the decoration of bookbindings since the middle of the 19th century. (128 , 262 , 347 )