Re: Reaction of silk woven rug while testing with solvents
Thank you for the point raised. I cannot think of it being rayon as it a 16th c. famous rug published and researched thoroughly. There are some recently re-warped areas but I did not wet those.
Konstantinos Chatziantoniou
Textile and Paper Conservator
Museum of Islamic Art
Al Corniche
Doha
P.O.Box 2777
Qatar
email: khatziantoniou@xxxxxxxxxx
Tel: +974 6980254
----------------------------------------
> Date: Tue, 29 Jul 2008 11:21:48 -0400
> From: KKiefer@xxxxxxxxxxxxx
> Subject: Re: Reaction of silk woven rug while testing with solvents
> To: TEXCONS@xxxxxxxxxxxxxxxxxx
>
> Are you sure the areas you tested are 100% silk. Rayon sometimes
> responds this way when wetted. Just a thought...
>>>>>>>>>>>>>>>><<<<<<<<<<<<<<<
> Kathleen Kiefer
> Senior Conservator of Textiles
>
> Indianapolis Museum of Art
> Virginia B. Fairbanks Art & Nature Park
> Oldfields-Lilly House & Gardens
> 4000 Michigan Road
> Indianapolis, IN 46208-3326
> kkiefer@xxxxxxxxxxxxx
> 317-923-1331 x155 - phone
> 317-926-8931 - fax
>
>
> -----Original Message-----
> From: Textile Conservators [mailto:TEXCONS@xxxxxxxxxxxxxxxxxx] On Behalf
> Of K Hatziantoniou
> Sent: Tuesday, July 29, 2008 7:49 AM
> To: TEXCONS@xxxxxxxxxxxxxxxxxx
> Subject: Re: Reaction of silk woven rug while testing with solvents
>
> Dear all,
>
> I just came across something I have not seen previously and I need your
> opinion:
> Before treating I tested a silk Islamic rug (16th c, very light-weight,
> extremely tight woven) for a possible solvent cleaning with IMS, acetone
> and also a 0,3% of Dehyphon in deionised water. The very soft rug became
> extremely rigid in these tested areas. In two days these areas became
> softer but never returned to their previous state. Unfortunately the rug
> has been purchased in auction and this part of its previous restoration
> treatment remains unknown (no documentation record exists). It must have
> been treated in USA considering its previous owner, in the 60s or 70s.
> After brief consultation the question of fire protection spraying of the
> rug was raised.
>
> Does anyone knows why a 100%silk rug may react on all the above solvents
> and washing detergent in such an extreme way?
>
> Many thank you for your time and help
>
> Konstantinos Chatziantoniou
> Textile and Paper Conservator
> Museum of Islamic Art
> Al Corniche
> Doha
> P.O.Box 2777
> Qatar
> email: khatziantoniou@xxxxxxxxxx
> Tel: +974 6980254
> _________________________________________________________________
> 100's of Nikon cameras to be won with Live Search
> http://clk.atdmt.com/UKM/go/101719808/direct/01/
>
> smtp.imamuseum.org made the following annotations
> ---------------------------------------------------------------------
> NOTICE: This email message is for the sole use of the intended recipient(s)
> and may contain confidential and privileged information. Any unauthorized
> review, use, disclosure or distribution is prohibited. If you are not the
> intended recipient, please contact the sender by reply email and destroy all
> copies of the original message.
> ---------------------------------------------------------------------
_________________________________________________________________
Find the best and worst places on the planet
http://clk.atdmt.com/UKM/go/101719807/direct/01/