For those using Surfonic JL-80X as a replacement for Triton XL-80N, the
CMC is 88.5ppm (which compares with the reported CMC of XL-80N of about
86 ppm). So one can continue to use the replacement product at similar
concentrations.
The CMC was measured for us by request by David Coffey, Research
Chemist, Huntsman Advanced Technology Center. The technical support
phone number there is 281-719-7780.